ESAB Introduces Dual Shield X-Series Flux-Cored Wires

Florence, SC – ESAB Welding & Cutting Products introduces its newest family of flux-cored wires, the Dual Shield X-Series. These new wires offer advancements that make this new series much more forgiving than traditional flux cored wires, especially for less experienced welders. Dual Shield X wires give the welder a wider range of operating parameters than traditional wires in the same class, high deposition rates, fast travel speeds, flat bead profile, limited spatter and extremely easy slag removal.

The X-Series includes wires for use with CO2 or mixed gases, and wires for flat, horizontal and all-position welding. These wires meet requirements for multiple weld procedures ranging from general fabrication to critical welding applications. Key industries include civil construction, ship building, heavy equipment, offshore oil rigs and rail car fabrication.

With more than 100 years of experience, ESAB Welding & Cutting Products is one of the world’s largest and most skilled manufacturers of welding and cutting equipment and welding filler metals. Ensuring customer satisfaction, a wide range of ESAB products carry the 100% Satisfaction Guarantee. Recognized as the technological leader in the industry, ESAB is committed to providing customized solutions for their customers. For more information on the new Dual Shield X-Series wires, visit www.esabx.com.

undefined